Home / Products / Bimetallic Wear Plates
Wear Parts

Bimetallic Wear Plates (BT-CW)

A hard wear layer on a tough steel backing, cut, drilled and formed to your drawing - for chutes, hoppers and transfer points.

Overview

A bimetallic wear plate - often written bimetal wear plate - is a composite steel plate: a hard, abrasion-resistant layer bonded to a tough structural steel backing. BT-CW is ours. It is built for surfaces where material slides continuously and a plain steel liner wears through - chute linings, hopper walls, transfer points, discharge spouts and loader or excavator wear surfaces.

The two layers do different jobs. The wear layer faces the material stream and resists sliding abrasion; the backing absorbs impact, carries the bolt loads and holds the plate flat against the structure. That combination is why a bimetallic plate can be thinner than a cast wear block and still be bolted to a chute wall.

Two names are often confused with it. A bimetal strip is the thin two-metal strip used in thermostats and switches. Copper-clad steel is a clad metal chosen for conductivity or corrosion resistance. Neither is a wear plate. If your drawing is for a clad metal rather than a wear liner, say so and we will point you to the right supplier instead of quoting a wear plate.

Where a bimetallic plate is the right choice

Composite wear plate, bimetallic plate: the same thing?

In the trade the two names describe the same construction: a hard wear layer welded onto a structural steel backing. We call ours BT-CW; buyers often ask for a "composite wear plate" or a "bimetal plate", and both arrive at the same sheet.

Build-ups run 6+4, 8+6 and 10+10 mm, and hardness is checked on every plate with a Leeb tester - typically 54-64 HRC for this family. If your enquiry says "composite wear plate", nothing needs translating: send the drawing and the duty, and the build-up follows from that.

Specifications

TypeBT-CW bimetallic (composite) wear plate
ConstructionHard wear layer bonded to a structural steel backing
Wear-face hardnessTested on every plate with a Leeb tester; typically 54-64 HRC for this family - take the exact value from the specification
Build-upQuoted as wear layer + backing, e.g. 6+4, 8+6 or 10+10 mm; confirmed against duty and drawing
BackingCarbon structural steel, grade to drawing
Plate sizeCut to drawing; large plates available
FixingBolt holes, countersunk holes, weld-on, plug weld
FlatnessChecked against the structure before dispatch
Lead time7-20 days, confirmed with the quote

Choosing the build-up

The build-up is written as wear layer + backing. The wear layer is the sacrifice; the backing carries the load and the fixing. Typical industry build-ups look like this - use them as a starting point, not a substitute for the duty:

Build-up4+4 mm - light sliding abrasion, small chutes, low headroom.
6+4 mm - general chute and hopper linings, moderate impact.
8+6 mm - the common heavy-duty request: coarse material, longer intervals between stops.
10+10 mm - high wear allowance, large lumps, structures that can carry the weight.

Two checks decide more than the number. First, the wear rate of the liner being replaced: if it lasted 4,000 hours and you want 12,000, you need roughly three times the wear allowance, not a thicker backing. Second, the structure: bolt size, hole spacing and the weight the wall can carry. Send both and the build-up can be settled on the drawing.

Bimetallic, chromium carbide or white iron?

Bimetallic plateSolid wear layer on a structural backing. Good where the liner sees sliding abrasion plus moderate impact, and where it must be formed, drilled and bolted. The all-round choice for chutes and hoppers.
Chromium carbide overlayCarbide-rich weld overlay on mild steel. Very high abrasion resistance at the surface; less tolerant of impact and of tight forming. Strong where the duty is pure sliding abrasion.
White ironCast or laminated high-chrome iron. Excellent abrasion resistance, brittle under impact, and usually fixed as blocks or tiles rather than drilled plates.

Full comparison: bimetallic vs chromium carbide vs white iron →

CORC-g® and BT-CW: what the comparison covers

CORC-g® is the compound steel wear plate made by Josua CORTS Sohn GmbH in Germany. It is a registered trademark of CORTS, and it is the name many mill and sinter-plant drawings carry because that is the plate the OEM fitted. BT-CW is our own designation for a plate of the same construction: a compound steel bonded as two solid metals, with a hardened tool-steel wear face (about 25% of the section) and a tough, low-carbon backing (about 75%), supplied as an independent CORC-g®-equivalent alternative, and made to CORC-g® drawings where the drawing specifies it. We are not a CORTS agent, distributor or licensee, and BT-CW is not a CORTS product.

The three grades line up with the three duties CORC-g® drawings usually describe - equivalent in construction and duty, not in origin:

BT-CW-BWear face 58-60 HRC; hard layer about 25% of the section (6 mm on a 25 mm plate), low-carbon backing. General sliding abrasion: chutes, hoppers, transfer points. The standard-wear equivalent.
BT-CW-BSWear face 54-58 HRC; hard layer about 25% of the section, stainless backing. Wet, salty or corrosive material. The stainless (rostfrei) equivalent.
BT-CW-BEWear face 60-64 HRC; hard layer about 25% of the section (8 mm on a 32 mm plate), low-carbon backing. Coarse lumps, high impact, mill housings and bearing seats. The heavy-wear equivalent.

Bond strength is 500-600 N/mm² on the interface shear test for all three grades. What we do not claim is identical chemistry or identical service life: the wear layer is a high-alloy tool steel to our own specification, and life depends on the duty. Where a drawing calls for CORC-g®, send the hardness and case depth written on it - for example 58-60 HRC at 7.5 mm - and we check the section against those figures before quoting.

What to send with an enquiry

What we check before dispatch

Product images

Typical applications

Chutes and hoppers

Liner layout, fixing and build-up for transfer points.

Read the guide →

Mining and aggregate handling

Discharge spouts and bins

Excavator and loader wear parts

Cement and steel plant liners

Specifying, fitting and checking a BT-CW plate

A wear plate is a consumable, so start from the duty and the replacement interval, not from the grade name. Five decisions set the plate:

Fitting is where most plates fail early. Support the plate over its full area, keep fixings away from the edge, allow for thermal movement on long runs, and tighten to the specified torque in the sequence on the drawing. A plate that is pulled down onto a high spot will crack at the hole or wear through at the gap.

Before dispatch we check the wear-layer hardness, the bond line, the hole pattern and the overall dimensions against the drawing. If the plate is cut to a template, the template is checked first.

Working out the wear allowance

The build-up is a wear allowance, not a strength grade. Two measurements settle it.

  1. Measure the liner being replaced. Take readings at the discharge point, the centre of the plate and the area behind the first impact. The difference between the original thickness and the thinnest reading is the wear that occurred over the service interval.
  2. Convert it to a rate. Divide the worn millimetres by the hours or tonnes the liner ran. A liner that lost 4 mm in 6,000 hours wears at about 0.67 mm per 1,000 hours; if the next interval is 12,000 hours, the wear layer needs about 8 mm plus a margin.

Then check the structure. A thicker backing adds weight and moves the bolt load; it does not slow wear. If the existing bolts and wall are near their limit, keep the backing and increase only the wear layer. Where impact is the dominant mechanism, the backing does more work than the wear layer: a 6+6 plate can outperform a 10+4 plate on a transfer point that sees lumps.

Installation sequence

  1. Dry-fit the plate on the structure before drilling. Check that it seats over its full area and that no high spot holds it off.
  2. Mark holes from the structure, not from the old plate. Old plates distort and their holes move.
  3. Support the plate over its full area. A plate bridged across a gap flexes under load and cracks at the fixings.
  4. Bolt from the centre outward so the plate is pulled down evenly.
  5. Torque in the sequence on the drawing. Re-check after the first heat cycle or the first week of running.
  6. Apply plug welds, if specified, after the bolts are torqued - not before.
  7. Check gaps between plates. Material entering a gap lifts the edge and starts edge wear.
  8. Record the plate ID and the hardness reading that ships with it, so the next replacement can be compared like for like.

Failure modes and what they tell you

What you seeUsual causeWhat to change
Wear-through in one patchMaterial stream concentrated in one line; local plate too thin for that pointAdd a thicker section or a deflector at that point - not a thicker plate over the whole area
Edge lifted or curledEdge unsupported; fixings too far from the edge; thermal movement restrainedSupport the edge, move fixings inward, allow movement on long runs
Bolt holes elongatedBolts lost torque; plate moving; hole oversize or washer too smallRe-torque to spec, use larger hardened washers, ream the hole if it has opened
Crack from a hole or weldPlate pulled down onto a high spot; weld restraint; hole too close to the edgeFlatten the seat, change the weld sequence, increase edge distance
Wear in the gap between platesGaps too wide; plates not pulled tight; flow running across the jointClose the gap, overlap in the direction of flow, check the fixing layout
Bond-line separationImpact beyond the design duty, or a manufacturing defectReview the duty and the impact point; check the hardness and bond record for the batch

Cutting, drilling and forming

BT-CW is supplied cut to drawing, but site modifications are common. Cut with plasma or waterjet and keep the heat-affected zone away from the bond line; do not flame-cut across the wear face. Drill from the backing side with carbide tooling, and countersink before the hole is opened up. Bend direction and radius should be agreed on the drawing: bending across a hole, a weld or a previously bent line concentrates stress and is a common source of cracking. If a plate has to be re-formed on site, anneal or stress-relieve only after checking with us, because the wear layer and the backing respond differently to heat.

FAQ

Related products

Related: CORC-G, the two-layer liner for mill housings and chocks

Need a quote or a custom part?

Send your drawing, sample photo or specification - we reply within 1 business day.

Request a Quote