Home / Products / Babbitt Bearing Shells & Oil-Film Bearings
Babbitt bearing shells

Babbitt Bearing Shells & Oil-Film Bearings

The core pivot of heavy-duty equipment

Babbitt (white metal) bearing shells and oil-film bearings for heavy-duty rotating equipment - cast, bonded and machined to drawing, in tin/lead alloys.

Overview

Babbitt bearing shells - also called white-metal bearings or oil-film bearings - are the pivot a machine actually turns on: every ton of load on a rotary kiln, mill, turbine or reducer passes through them. We supply these shells cast and machined to the original drawing, or reverse-engineered from a sample or site measurement, in tin-based and lead-based Babbitt, solid or bonded to a steel or cast-iron shell back where the duty requires it.

Further reading: Babbitt Bearing Shells Explained →

Product images

Key features

Specifications

Typical partsBearing shells, oil-film bearings, bushes and thrust pads
MaterialTin-based and lead-based Babbitt (white metal)
GradesZSnSb11Cu6, ZSnSb8Cu4, ZSnSb4Cu4, ZSnSb12Cu6Cd1, ZSnSb12Pb10Cu4, ZPbSb16Sn16Cu2, ZPbSb15Sn10, ZPbSb15Sn5, ZPbSb10Sn6
ConstructionSolid, or Babbitt bonded to a steel / cast-iron shell back
Lining thickness1-5 mm typical, to drawing
ProcessCasting, tinning and bonding, machining and fitting to contact
SizesUp to 1,500 mm diameter, larger on request
Bore and fitMachined to drawing, including clearance and contact
LubricationOil grooves, oil ways, oil holes and keyways to drawing
Bond checkLining inspected for sound bonding before dispatch
MOQ1 piece
Lead time10-20 days

Typical applications

Cement rotary kilns & mills

Steam and gas turbines

Gearboxes and reducers

Pumps and compressors

Large rotating equipment refurbishment

Tin-based or lead-based Babbitt?

The base metal decides how the shell behaves in service, and it is the first choice you make - before size, before clearance. This is how the two families compare for the grades we cast:

Base metalTin-based BabbittLead-based Babbitt
Grades we castZSnSb11Cu6, ZSnSb8Cu4, ZSnSb4Cu4, ZSnSb12Cu6Cd1, ZSnSb12Pb10Cu4ZPbSb16Sn16Cu2, ZPbSb15Sn10, ZPbSb15Sn5, ZPbSb10Sn6
Melting pointAbout 220-245 °C (430-470 °F)About 235-250 °C (460-480 °F)
Continuous dutyAbout 130 °C, up to about 150 °C peakSimilar, with lower load capacity
Load capacityHighModerate
CorrosionGoodPoorer - sensitive to water and acidic oil
Relative costHigher (tin content)Lower
Typical useTurbines, generators, large pumps, high-speed shaftsGeneral industrial bearings where cost drives the choice

Rule of thumb: for continuous, well-lubricated, high-load or high-speed duty, choose tin-based. Choose lead-based where the duty is moderate and cost matters more than load capacity, and keep water and acidic oil away from it. The full figures, including the ASTM B23 melting-point table, are in Babbitt Bearing Shells Explained.

Lining thickness and the bond

The lining is deliberately thin - commonly 1 to 5 mm. A thin layer carries load better, sheds heat faster and fatigues far more slowly than a thick one, which is why the thickness on the drawing is a design decision, not a casting convenience. Where there is no drawing, we set it from the shaft diameter, the load and the speed.

The lining is bonded, not simply poured in place. The shell back is cleaned and tinned, the Babbitt is cast against it, and the finished lining is checked for sound bonding before it is machined. A void at the interface is where a shell fails: the lining heats locally, softens and wipes, and the shell that looked fine on the bench takes the shaft with it. The casting, tinning and bond-test sequence is described in how Babbitt bearing shells are made.

Clearance, contact and checking

A shell is only half a bearing. What the shaft actually runs on is the oil film, and the film is set by clearance, so the bore is machined to the drawing rather than to a nominal size. The oil ways matter just as much: grooves, oil holes and keyways have to land where the drawing puts them, or the shell starves.

Three things are worth checking on delivery - the bore diameter and clearance, the contact pattern after bedding in, and the position of the oil ways. We check the shell dimensionally before dispatch and can supply a material certificate on request.

How to order a babbitt bearing shell

Send whatever identifies the part and we work from it:

If you are raising an RFQ, our guide to choosing a babbitt bearing shell manufacturer covers the alloy, bonding and tolerance questions worth putting in it.

Frequently asked questions

What is a babbitt bearing shell?

A babbitt bearing shell is a bearing in which a thin layer of Babbitt metal (white metal) is cast onto a steel or cast-iron back, or used as a solid bush, then machined so the shaft runs on an oil film. It is the pivot under every tonne of load on a kiln, mill, turbine or reducer.

What is the difference between tin-based and lead-based Babbitt?

Tin-based Babbitt carries more load, resists corrosion better and costs more. Lead-based Babbitt is cheaper and melts at a slightly higher temperature, but it carries less load and is sensitive to water and acidic oil. Tin-based is the choice for turbines, generators, large pumps and high-speed shafts.

At what temperature does babbitt bearing metal melt?

Tin-based Babbitt melts at about 220-245 °C (430-470 °F) and lead-based Babbitt at about 235-250 °C (460-480 °F). The working limit is far below that - the lining softens long before it melts, and about 130 °C continuous with 150 °C peak is the usual ceiling.

How thick is the babbitt lining?

Commonly 1 to 5 mm. Thin is deliberate: a thin lining carries load better, sheds heat faster and fatigues more slowly than a thick one.

Can you make a shell from a sample or a site measurement?

Yes. We reverse-engineer from a worn shell, a photo with dimensions or a site measurement, and work to your drawing where one exists.

What is the minimum order and the lead time?

One piece, and typically 10-20 days depending on size and grade.

Need a quote or a custom part?

Send your drawing, sample photo or specification - we reply within 1 business day.

Request a Quote